Place of Origin: | China |
Brand Name: | JIMA |
Certification: | ISO |
Model Number: | 3104 |
Minimum Order Quantity: | negotiation |
---|---|
Price: | negotiation |
Packaging Details: | wooden carton pack |
Delivery Time: | 15-30 days |
Supply Ability: | 10000 ton per monh |
Alloy: | 3104 | ID: | 405MM,505MM,605MM |
---|---|---|---|
Standard: | GB/T9106.1-2009 | Application: | Can Body And Can End |
Temper: | H19,H48 | Item: | 3104 H19 Aluminum Coil For Can Body Stock Delivery Fast |
Thickness: | 0.270mm | Packaging: | Wood |
Highlight: | H19 Aluminum Coil Stock,H48 Aluminum Coil Stock,A3104 aluminum alloy coil |
Aluminum Alloy Coil for Body Stock A3104 Temper H19
Aluminum coil 3104 h19 for can body technical specification
Alloy | Temper | Thickness and tolerance | Width and tolerance |
3104 | H19 | 0.279±0.005mm | 1491.79-0/+1.5mm |
1. Requirement
1.1Alloy. Temper. Dimension tolerance
Aluminium coil 3104 Chemical composition
Alloy | Chemical composition (not more than) | |||||||||||
Fe | Si | Cu | Mn | Mg | Ti | Zn | Ga | V | Others | Al | ||
each | total | |||||||||||
3104 | ≤0.8 | ≤0.6 | 0.05-0.25 | 0.8-1.4 | 0.8-1.3 | ≤0.1 | ≤0.25 | ≤0.05 | ≤0.05 | 0.05 | 0.15 | Other |
Aluminio 3104 h19 Mechanical property and Process property
Mechanical property |
Process Property |
|||
Tensile Strength Rm |
Yield Strength Rp0.2 |
Post Baked Elongation A50mm/% |
Post Baked Yield Strength (205℃/10min 400°F/10min) |
Earing /% |
≥293MPa | 270-305MPa | ≥4.0 | 255-288MPa | ≤4 |
1.5 Oscillation and Telescoping
The oscillation shall not be more than 2mm,and telescoping no more than 5mm.
1.6 Edge camber
The edge camber shall not be more than 1mm maximum in 1000mm on the strip
1.7 Flatness
The gap between the strip and the flat surface should less than 6mm, the amount of wave in one meter length should no more than 3.
1.8 Surface Roughness:Ra:0.30~0.60 μm.
2. Appearance quality
The surface should be clean, even texture. Defects which may affect the material processing are forbidden, such as serious scratches, speckles, corrosions, oil stains, air entrapments, holes, peeling, inclusions, metal and nonmetal inclusions, black streaks or black lines.
2.2. The trimmed coil must be without cracks,clean cutting edge
2.3. The coils should be tight and even on the edges ,no splice
Can supply
aluminium can body stock
aluminio 3104 h19
bobina de aluminio para 3104 h19 cuerpo puede
bobina de aluminio 3104 h19
aluminum coil 3104 h19 for can body
aluminium coil 3104
Surface Lubrication
Post Lube | Post Lube Control Amount |
Henkel DTI PL-A |
250±125mg/m2/side 25.0±12.5mg/ft2/side |
Body Stock Coil
Aluminum Alloy 3104 H19 for Can Stock
Aluminum Coil for Can Body 3104
Aluminum Coil 3104 H19 for Can Body
Aluminio 3104 H19
Can Body Stock
Coil packing type Paperless packaging
Application:
Packing Photos
Contact Person: Annie
Tel: Whatsapp:+8615000729029